SUPERALLOYS/ALLOYS: NITINOL:40-45% titanium/55-60% nickel 110k-124k t.s.[tensile strength rockwell:42-52 *TUNGSTEN ALLOY 15C: for percussion applcations subject to medium to heav impact *ZIRCONIUM COPPER N-4 0.25 Zr/bal.Cu 3k T.S.[75*F] high strength and conductivity at high temperatures. *ZIRCONIUM ATR: 0.5 Cu/0.5 Mo/bal. Zr 45k T.S.[at 600*f] corrosion resistant at high temperatures[from CO2] for nuclear reactors. *LOIRE SP20: for exhaust valves,jet engine components/corrosion and heat resistant to 1000*c. *RMI 6A-4V ELI:
for high pressure cryogenics
-320*F=220k T.S./-423*F=65k T.S./205k T.S.
Ti alloy

*STAUFFER 90Ta-10W:
cold drawn=160k T.S.
or flame barriers,rocket engine parts,nozzles
usefull in the temperature range of -200*F to 5200*F

*PROPLATINUM:
platinum substitute for corrosion resistance

*TURBISTON BRONZE:
55 CU/41 Zn/2 Ni/1 Al/0.84 Fe/0.16 Mn
for pistons,
highly resistant to sea water/also called a brass

*UDIMET 71:
0.05 C/18 Cr/18 Fe/3 Mo/5.2 Cb/1 Ti 0.06 Al/0.004 B/bal Ni
190k T.S.[70*F]/170k T.S.[1200*F]
-423*F to 1300*F
applications:for components of gas turbines,missile and booster assemblies

*UDIMET 625:
0.05 C/22 Cr/3 Fe/9 Mo/4 Cb/0.2 Ti/0.2 Al/bal. Ni
103k T.S.[1200*F]
good oxidation and corrosion resistance
high strength from cryogenic to 2000*F

*VIRGO 1:
for molten salt containers
type 410
corrosion resistant
most suitable as a coating

*SILVER BEARING COPPER 114:
electrical conductivity:100

*MAGNESIUM LA 142:
at 200 *F=15.3 T.S.
for armoured ordinance vehicles

*TUNGSTEN ALLOY 30H:
forparts subjected to extra heavy impact

*TUNGSTEN ALLOY 15C:
medium to heavy impact resistance

*NICKEL "C":
69k T.S.
best corrosion resistance to salt solutions

*SUPER RADIOMETAL:
58k T.S.
for magnetic shields/soft magnet/hgh permeability and low losses

*BERYLCO 717:
age hardened:145k T.S. min.
rockwell:c29
for piping,high velocity heat exchangers,hydrophone parts
high sea water corrosion resistance

*MOLYBDENUM PERMALLOY 4-79:
for high frequency-high pemeability-high resistance
81% Ni

*COVANDUR:
for electrical equipment,sonar,ultrasonic transducers
soft magnet/high magnetic saturation

*CUPRO-NICKEL 30% 715:
cold rolled 58k-90k T.S.
good corrosion resistance to high velocity salt water
for heat exchanger tubes and sheets

*CARBALOY 268:
490 T.S.
87.0 rockwell
high shock resistance for mining

*COMMERCIAL BRONZE 25:
90 Cu/10 Zn
for weather stripping

*CO-NETIC AA:
57k T.S.
for electrostaic shielding

*CO-NETIC B:
58k T.S.
for magnetic shielding

*ZURCO NO. 25:
25-30 Cr/0.01 C/bal. Fe
rustless steel
for continuous heat up to 2200*F

*HYFLUX ALNICO 4:
coercive force:1400 oersteds
residual induction:10,500 gausses
for straight field focusing devices,motors,spac age applications
permanent magnet/resists demagnification

*IMPHY IR:
for cutting tools,drills,lathes
high red hardness

*JOSYLIN SAINLESS TYPE 615:
140k T.S.
for jet engine parts
magnetic

*NICKEL VAC L-605:
55k T.S.[1500*F]
oxidation and corrosion resistance/high strength above 1600*F
for afterburners,igh temperature valves and springs
-------------------------------------------------------------------------------------------------
*NITINOL 55:
55% nickel/balanced titanium
120k T.S.
rockwell 50

*STAINLESS STEEL A:
260k T.S.
rockwell 50

*TITANIUM EP 90-10:
20k T.S.[70*F]/150k T.S.[800*F}

*TITANIUM 314A:
139k T.S.

*TITANIUM 371:
148k T.S.
for high temperature applications to 1000*F

*SUPERTHERM:
35 Ni/26 Cr/15 Co/5 W/1.6 Si/0.5 C/bal. Fe
75k T.S.
heat resistance up to 2300*F

*TUNGSTEN RHC:
4 Re/0.35 Hf/0.25 C/BAL. W
75 k T.S. minimal at 3500*F
high heat and oxidation resistance

*RHENIUM:
70 k T.S.
99.5% Re
for electroplating

*ZIRCONIUM COPPER 150:
99.83 % Cu/0.17% Zr
93% electrical conductivity
corrosion resistant

*HIDUMINIUM R.R. 56:
60k-72k T.S.
automobile connecting rods,Rolls Royce,supercharger motors

* Nitinol: [1] 40-45% Ti/ 55-60% ni [2] 110,000-124,000 T.S./ 40,000- 50,000 Y.S. [3] Rock A 42-45 [4] Nonmagnetic, corrosion resistant Nitinol 55 [1] 55 Ni/ bal Ti [2] 120,000 T.S./ 50,000 Y.S. [3]Rock A 50 [4] non magnetic, corrosion resistant Stainless steel A: [1] 260,000 T.S. [2] 510 brn [3] corrosion resistant Tantalum Bronze: [1] 698,700 T.S./ 44,000 Y.S. [2] corrosion resistant KYONKhm: [1] 368,000 T.S./ 248,000 Y.S. [2] up to 400*C service [3] 88 Rock AMCARB D-50: [1] 425,000 T.S. [2] 15 co/ 85 wc [3] A87 Rock [4] wear/ abrasion resistant ARNOX-1: [1] permanent magnet. Non conducting. non orienting Beryllium Malleable: [1] For x-ray windows [2] 99.8 Be/ 0.2Ti Carpenter Hy-Sat 48 FM; [1] ultrasonic transducer material [2] 0.04 C/ 0.80 Mn/ 0.40 Si/ 49.0 Co/ 1.9 V/ 0.20 Se/ bal. Fe Carprnter Stainless 304+B: [1] shielding for nuclear reactors [2] 100,000 T.S./ 50,000 Y.S. Carbaloy HM-1 Hevimet: [1] 300,000 T.S. [2] C25 Rock [3] 90% W/ 7.5% Ni/ 2.5 Co [4] radiation shielding. Vibration damping Rynalloy: [1] m-!211 [2] Ball socket/ joints in aircraft exhaust systems. [3] for use up to 1,800*F Sandavik 11R51: [1] 341,000 T.S. [2] For springs for instruments. High fatigue life and tensile Strength[T.S.] Scholler Masoy Superior: [1] 80,000 T.S. [2] B78 Rock [3] Type 316 Stainless Steel [4] For chemical plant equipment Semalloy No.A978: [1] melting range: 2,876*F-3,110*F [2] Au and Pt Semalloy No. 3900: [1] melting range: 5,425*F for M1729 [2] Ta SEmalloy No. 3910: [1] melting point: 5,756*F [2] Rh SGS Tantalum: [1] M-1624 [2] 11Ta + Yttrium [3] 300% stronger than tantalum at 1,650*C [4] used in electric/ electrical components, aerospace ,and nuclear systems Tizit FM: [1] M-1246 [2] Wc/ TiC/ TaC/ Co/ [3] For cutting tools and dies No. 1040 Alloy: [1] For electrical equipment. Magnetic alloy. Achorn T2 High Speed Alloy: [1] tungsten type high speed steel ACIPCO HK: [1] completely austentitic stainless. Service to 2,000*F APA MAS TITAN 80: [1] finish machining and boring alloys and superalloys. A.E.B. Stainless: [1] for razpor blades, surgical instruments. Corrosion resistant Aeralloy 23: [1] For electrical contacts. Resists arc corrosion AGMOLITE: [1] For electrical contacts for circuit breakers. A-l 18 NiCoMo[250]: [1] Rocket cases, aircraft landing gears Alcoa 5456: [1] For overhead cranes. ALCOLOY R 688: [1] Excellent corrosion resistance, high strength. [2] Forrelay springs and electric terminals. Allegheny A-286: [1] jet engine, supercharger parts, and after burners for jets. *Allegheny LUDLUM-LXX: [1] 454,000 bond strength [2] Type 1 high speed steel. High ed hardness Allegheny Type 203 EZ: [1] austentitic Stainless [2] Free cutting [3] 135,000-208,000 T.S. Alloy CB-7: [1] 60,800 Y.S. [2] high temperature applications. High temperature strength to 2,000*F Alloy L.T.C.: [1] For resistors. High electrical resistance Alloy W.6.: [1] For spark plug electrodes. Resists high temperature corrosion, ALL-PRO: [1] For overlay orbuildup on scrapers, loaders, dozer bits, blades, shovels, buckets. [2] good abrasion resistance ALMAR 20: [1] For bolts, cryogenic and high temperature equipment. [2] Maraging steel . Shock resistant [3] 253,000- 265,500 T.S. *ALNICO5: [1] cast permanent magnet material [2] M-60 for high energy *ALNICO v111: [1] For Focusing of elecxtron beams *ALNIFER: [1] for electron tubes Allegheny Z5-12S: [1] M-1. For stainless steel castings [2] Resists H2SO4/ HNO4/ Acetic acids [3] cast (0K T.S./ 40K Y.S. [4] 0.11 max C/ 22-26 Cr/ 12-14 Ni/ bal Fe Allegheny 88X: [1] M-1 [2] For large electrical transformers, switchboard parts [3] non magnetic. high electrical reesistivity [4] 0.2- 0.3 C/ 10-12.5 Mn/ 7- *.5 Ni/ Bal Fe *Allegheny Am 357: [1] M-1 [2] sheet 309K T.S./ 303K Y.S./ at 1,000*F= 158K T.S./ 141K Y.S. [3] For valves, pressure tanks, aircraft jet engine parts. [4] semi- austentitic Stainkess steel [5] 0.21- 0.26C/ 0.50- 1.25 Mn/ 13.5-14.5 Cr/ 4.0- 5.0 Ni/ 2.5- 3.25 Mo/ 0.07- 0.13N/ Bal Fe Allegheny LUDLUM 129: [1] M-1 [2] ht.tr. 322K T.S./ 265K Y.S. [3] For tools, bearings for high temperature applications. [4] Stainless. high corrosion resistant [5] 0.7 C/ 0.3 Mn/ 1.0 Si/ 12 Cr/ 5.25 Mo/ bal Fe Allegheny 2000: [1] M-1216 [2] For plating anodes [3] 100 NI Alloy W.5.: [1] m-121 [2] For high temperature corrosion resistant spark plug electrodes [3] 4 Si/ 0.5 Mn/ bal Ni ALLVAC 18-15B: [1] For neutron control rods, atomic energy uses. [2] Austenitic Stainless [3] 0.01C/ 18Cr/ 15Ni/ 0.8B/ bal Fe [4] M-1490 ALMET 17-7PH: [1] Ht.tr.[ heat treated] 244K-345K T.S./ 234K-340K Y.S. [2] For springs, cli[s, aircraft parts [3] Stainless. M-248 [4] 0.09 max C/ 17Cr/ 7Ni/ 0.75-1.25Al/ bal Fe